Include Product Page Fe-doped SrTiO3
| LINEAR FORMULA: |
Fe-doped SrTiO3
|
| PURITY: | >99.99% |
| CRYSTAL ORIENTATION: | (100), (110) & (111) |
| GROWTH METHOD: | Czochralski Method |
| DOPING CONCENTRATION | Fe 0.05% |
| CRYSTAL STRUCTURE: | Perovskite |
| LATTICE CONSTANT: | a=b=3.905 A. c=3.905 A |
| MELTING POINT (°C): | 2100 degsC |
| THERMAL EXPANSION COEFFICIENT (/K): | a11=8.0 x 10^-6/K, a33=9.0 x10^-6/K |
| HARDNESS: | 6 |
| MOLAR MASS (G/MOL): | 183.5 g/mol (including dopant) |
| DENSITY (G/CM3): | 5.00 g/cm3 |
| REFRACTIVE INDEX: | n=2.43 (632.8nm) |
| SPECTRAL TRANSMISSION RANGE: | 400-6000 nm >80% (632.8 nm) |
| SIZES: | 5x5mm & 10x10 mm + on request |
| TYPICAL THICKNESS: | 0.5mm |
| SIZE TOLERANCES: | +/- 0.1mm |
| THICKNESS TOLERANCES: | +/- 0.015mm |
| ORIENTATION PRECISION: | +/-0.5 degree |
| POLISHING OPTIONS: | SINGLE SIDED (1SP) OR BOTH SIDES POLISHED (2SP) |
| ROUGHNESS RA: | <0.5nm |